Electrical Engineering Wroclaw University of Technology

Electrical Engineering Wroclaw University of Technology 25 records found  1 - 10nextend  jump to record: Search took 0.00 seconds. 
1.
Temperature monitoring of metal oxide surge arresters / Chrzan, K L ; Hinrichsen, V. [ENY-ARTICLE-2013-343]
Varistor overtemperature above the ambient is an important state parameter of metal oxide surge arresters. [...]
http://zet10.ipee.pwr.wroc.pl/record/430/files/
Detailed record - Similar records
2.
Internal partial discharges test for metal oxide surge arresters / Chrzan, K L [ENY-ARTICLE-2012-327]
Proposals for testing of surge arresters performance under internal partial discharge stress by Sakshaug, Chrzan and Korycki have been presented. [...]
http://zet10.ipee.pwr.wroc.pl/record/414/files/
Detailed record - Similar records
3.
Termovision diagnostics of metal oxide surge arresters / Chrzan, K L [I07/2007/I-043] [ENY-ARTICLE-2008-187]
The surge arresters diagnostics based on infrared temperature measurement was evaluated. [...]
http://zet10.ipee.pwr.wroc.pl/record/238/files/
Detailed record - Similar records
4.
Behaviour of Insulators and Surge Arresters at Glogow Pollution Test Station / Chrzan, K L ; Haddad, A [I07/2005/I-005] [ENY-ARTICLE-2008-222]
The paper reports on the pollution performance of different insulators and surge arresters at Glogow test station from 1981 up to 2004. [...]
http://zet10.ipee.pwr.wroc.pl/record/277/files/
Detailed record - Similar records
5.
Influence of moisture and partial discharges on the degradation of high-voltage surge arresters. / Chrzan, K L [ENY-ARTICLE-2012-321]
This paper reports the influence of moisture and internal partial discharges on the degradation of metal oxide varistors in high-voltage surge arresters. [...]
http://zet10.ipee.pwr.wroc.pl/record/408/files/
Detailed record - Similar records
6.
Behaviour of Zinc Oxide Surge Arresters Under Pollution / Feser, K ; Kohler, W ; Qiu, D ; Chrzan, K L [ENY-ARTICLE-2008-214]
This paper presents results of pollution tests with A. [...]
http://zet10.ipee.pwr.wroc.pl/record/268/files/
Detailed record - Similar records
7.
Behaviour of zinc oxide surge arresters under pollution / Feser, K ; Kohler, W ; Qiu, D ; Chrzan, K L [I07/1990/I-114] [ENY-ARTICLE-2008-213]
This paper presents results of pollution tests with AC voltages which were carried out with a multi-unit zinc oxide arrester. [...]
http://zet10.ipee.pwr.wroc.pl/record/267/files/
Detailed record - Similar records
8.
Internal Arcing Test on Polluted High Voltage Surge Arresters / Chrzan, K L ; Kohler, W ; Feser, K [ENY-ARTICLE-2009-234]
A test to prove the performance of extremely non-uniform polluted single unit metal oxide (MO) and gapped arresters (SiCA) is presented. [...]
http://zet10.ipee.pwr.wroc.pl/record/293/files/
Detailed record - Similar records
9.
Pollution Performance of 110 kV Metal Oxide Arresters / Chrzan, K L ; Pohl, Z ; Grzybowski, S ; Kohler, W [ENY-ARTICLE-2008-216]
Pollution test results of single unit 110 kV metal oxide surge arresters with porcelain housing according to the solid layer and salt fog methods are presented. [...]
http://zet10.ipee.pwr.wroc.pl/record/270/files/
Detailed record - Similar records
10.
Diagnostics of high voltage metal oxide arresters procedure errors / Chrzan, K L ; Koehler, W [I07/2000/I-059] [ENY-ARTICLE-2008-193]
A technique has been described which can determine ac resistive current directly or by obtaining the watt loss of the test specimen and dividing by the true rms (trms) value or the applied voltage. [...]
http://zet10.ipee.pwr.wroc.pl/record/247/files/
Detailed record - Similar records

Haven't found what you were looking for? Try your search on other servers:
recid:430 in Google Books
recid:430 in Google Scholar
recid:430 in Google Web
recid:430 in INSPEC