Repozytorium Eny Politechnika Wrocławska

Repozytorium W. Elektrycznego Politechniki Wrocławskiej Znaleziono 28 rekordów  1 - 10następnykoniec  skocz do rekordu: Szukanie trwało 0.03 sekund. 
1.
Influence of moisture and partial discharges on the degradation of high-voltage surge arresters. / Chrzan, K L [ENY-ARTICLE-2012-321]
This paper reports the influence of moisture and internal partial discharges on the degradation of metal oxide varistors in high-voltage surge arresters. [...]
http://zet10.ipee.pwr.wroc.pl/record/408/files/
Rekord szczegółowy - Podobne rekordy
2.
Internal partial discharges test for metal oxide surge arresters / Chrzan, K L [ENY-ARTICLE-2012-327]
Proposals for testing of surge arresters performance under internal partial discharge stress by Sakshaug, Chrzan and Korycki have been presented. [...]
http://zet10.ipee.pwr.wroc.pl/record/414/files/
Rekord szczegółowy - Podobne rekordy
3.
Changes in varistors properties after radial field test / Jaroszewski, M ; Korycki, P ; Wieczorek, K ; Zakrzewski, J [ENY-ARTICLE-2008-179]
ZnO varistors are used in commercial surge arresters in high voltage application in the area of power engineering. [...]
http://zet10.ipee.pwr.wroc.pl/record/229/files/
Rekord szczegółowy - Podobne rekordy
4.
Internal Arcing Test on Polluted High Voltage Surge Arresters / Chrzan, K L ; Kohler, W ; Feser, K [ENY-ARTICLE-2009-234]
A test to prove the performance of extremely non-uniform polluted single unit metal oxide (MO) and gapped arresters (SiCA) is presented. [...]
http://zet10.ipee.pwr.wroc.pl/record/293/files/
Rekord szczegółowy - Podobne rekordy
5.
Behaviour of Insulators and Surge Arresters at Glogow Pollution Test Station / Chrzan, K L ; Haddad, A [I07/2005/I-005] [ENY-ARTICLE-2008-222]
The paper reports on the pollution performance of different insulators and surge arresters at Glogow test station from 1981 up to 2004. [...]
http://zet10.ipee.pwr.wroc.pl/record/277/files/
Rekord szczegółowy - Podobne rekordy
6.
Behaviour of Zinc Oxide Surge Arresters Under Pollution / Feser, K ; Kohler, W ; Qiu, D ; Chrzan, K L [ENY-ARTICLE-2008-214]
This paper presents results of pollution tests with A. [...]
http://zet10.ipee.pwr.wroc.pl/record/268/files/
Rekord szczegółowy - Podobne rekordy
7.
Termovision diagnostics of metal oxide surge arresters / Chrzan, K L [I07/2007/I-043] [ENY-ARTICLE-2008-187]
The surge arresters diagnostics based on infrared temperature measurement was evaluated. [...]
http://zet10.ipee.pwr.wroc.pl/record/238/files/
Rekord szczegółowy - Podobne rekordy
8.
Degradation and destruction of ZnO varistors caused by current pulses / Chrzan, K L ; Wroblewski, Z. [ENY-ARTICLE-2013-345]
Although the modern metal oxide elements are resistant to degradation caused by continuous operating voltage the degradation or destruction caused by current impulses, especially lightning currents, is still a serious problem. [...]
http://zet10.ipee.pwr.wroc.pl/record/432/files/
Rekord szczegółowy - Podobne rekordy
9.
Degradation of metal oxide varistors caused by electrical stresses / Chrzan, K L [ENY-ARTICLE-2013-350]
The degradation of ZnO elements under AC or DC operating voltage and impulse current is described. [...]
http://zet10.ipee.pwr.wroc.pl/record/437/files/
Rekord szczegółowy - Podobne rekordy
10.
Capacitance Changes in Degraded Metal Oxide Varistors / Jaroszewski, M ; Wieczorek, K ; Bretuj, W ; Kostyla, P [ENY-ARTICLE-2008-178]
ZnO based ceramics show a highly nonlinear current-voltage (I-V) characteristic due to intergranular layers at the boundaries of ZnO grains. [...]
http://zet10.ipee.pwr.wroc.pl/record/228/files/
Rekord szczegółowy - Podobne rekordy

Jeżeli nie znaleziono tego czego szukasz, spróbuj szukać na innych serwerach:
recid:408 w Google Books
recid:408 w Google Scholar
recid:408 w Google Web
recid:408 w INSPEC