Repozytorium Eny Politechnika Wrocławska

Repozytorium W. Elektrycznego Politechniki Wrocławskiej Znaleziono 16 rekordów  1 - 10następny  skocz do rekordu: Szukanie trwało 0.01 sekund. 
1.
Pollution flashover of single unit metal oxide arresters / Chrzan, K L ; Koehler, W. [ENY-ARTICLE-2013-342]
Flashover voltage of uniform and non-uniform polluted metal oxide arresters and their porcelain housings without internal parts was measured. [...]
http://zet10.ipee.pwr.wroc.pl/record/429/files/
Rekord szczegółowy - Podobne rekordy
2.
Internal Arcing Test on Polluted High Voltage Surge Arresters / Chrzan, K L ; Kohler, W ; Feser, K [ENY-ARTICLE-2009-234]
A test to prove the performance of extremely non-uniform polluted single unit metal oxide (MO) and gapped arresters (SiCA) is presented. [...]
http://zet10.ipee.pwr.wroc.pl/record/293/files/
Rekord szczegółowy - Podobne rekordy
3.
Pollution Performance of 110 kV Metal Oxide Arresters / Chrzan, K L ; Pohl, Z ; Grzybowski, S ; Kohler, W [ENY-ARTICLE-2008-216]
Pollution test results of single unit 110 kV metal oxide surge arresters with porcelain housing according to the solid layer and salt fog methods are presented. [...]
http://zet10.ipee.pwr.wroc.pl/record/270/files/
Rekord szczegółowy - Podobne rekordy
4.
Behaviour of zinc oxide surge arresters under pollution / Feser, K ; Kohler, W ; Qiu, D ; Chrzan, K L [I07/1990/I-114] [ENY-ARTICLE-2008-213]
This paper presents results of pollution tests with AC voltages which were carried out with a multi-unit zinc oxide arrester. [...]
http://zet10.ipee.pwr.wroc.pl/record/267/files/
Rekord szczegółowy - Podobne rekordy
5.
Behaviour of Zinc Oxide Surge Arresters Under Pollution / Feser, K ; Kohler, W ; Qiu, D ; Chrzan, K L [ENY-ARTICLE-2008-214]
This paper presents results of pollution tests with A. [...]
http://zet10.ipee.pwr.wroc.pl/record/268/files/
Rekord szczegółowy - Podobne rekordy
6.
Termovision diagnostics of metal oxide surge arresters / Chrzan, K L [I07/2007/I-043] [ENY-ARTICLE-2008-187]
The surge arresters diagnostics based on infrared temperature measurement was evaluated. [...]
http://zet10.ipee.pwr.wroc.pl/record/238/files/
Rekord szczegółowy - Podobne rekordy
7.
Diagnostics of high voltage metal oxide arresters procedure errors / Chrzan, K L ; Koehler, W [I07/2000/I-059] [ENY-ARTICLE-2008-193]
A technique has been described which can determine ac resistive current directly or by obtaining the watt loss of the test specimen and dividing by the true rms (trms) value or the applied voltage. [...]
http://zet10.ipee.pwr.wroc.pl/record/247/files/
Rekord szczegółowy - Podobne rekordy
8.
Internal partial discharges test for metal oxide surge arresters / Chrzan, K L [ENY-ARTICLE-2012-327]
Proposals for testing of surge arresters performance under internal partial discharge stress by Sakshaug, Chrzan and Korycki have been presented. [...]
http://zet10.ipee.pwr.wroc.pl/record/414/files/
Rekord szczegółowy - Podobne rekordy
9.
Changes in varistors properties after radial field test / Jaroszewski, M ; Korycki, P ; Wieczorek, K ; Zakrzewski, J [ENY-ARTICLE-2008-179]
ZnO varistors are used in commercial surge arresters in high voltage application in the area of power engineering. [...]
http://zet10.ipee.pwr.wroc.pl/record/229/files/
Rekord szczegółowy - Podobne rekordy
10.
Degradation and destruction of ZnO varistors caused by current pulses / Chrzan, K L ; Wroblewski, Z. [ENY-ARTICLE-2013-345]
Although the modern metal oxide elements are resistant to degradation caused by continuous operating voltage the degradation or destruction caused by current impulses, especially lightning currents, is still a serious problem. [...]
http://zet10.ipee.pwr.wroc.pl/record/432/files/
Rekord szczegółowy - Podobne rekordy

Jeżeli nie znaleziono tego czego szukasz, spróbuj szukać na innych serwerach:
recid:429 w Google Books
recid:429 w Google Scholar
recid:429 w Google Web
recid:429 w INSPEC