1.
Influence of profile on the pollution performance of ceramic long-rod insulators / Chrzan, K L [ENY-ARTICLE-2013-349]
The long rod insulators with different profiles were shown. [...]
http://zet10.ipee.pwr.wroc.pl/record/436/files/
Rekord szczegółowy - Podobne rekordy
2.
Artificial rain test of outdoor long rod insulators / Chrzan, K L ; Streubel, H [ISBN 978-0-620-44584-9] [ENY-ARTICLE-2009-279]
Due to the decrease of industrial contamination emission nearly the whole territory of Poland belongs to the pollution class light. [...]
http://zet10.ipee.pwr.wroc.pl/record/347/files/
Rekord szczegółowy - Podobne rekordy
3.
Pollution flashover of long rod insulators with different profiles. / Chrzan, K L ; Vokalek, J ; Sklenicka, V ; Petrusch, W ; et al [ENY-ARTICLE-2012-320]
Pollution test of four long rod insulators with different shapes were carried out according to flow on, salt fog and solid layer methods. [...]
http://zet10.ipee.pwr.wroc.pl/record/407/files/
Rekord szczegółowy - Podobne rekordy
4.
Pollution test station Glogow, twenty years of research / Chrzan, K L [ENY-ARTICLE-2008-215]
The evaluation of electrical stress of polluted outdoor insulators was carried out at the field test station located at a copper smelting plant Głogów in 1987 and 2002. [...]
http://zet10.ipee.pwr.wroc.pl/record/269/files/
Rekord szczegółowy - Podobne rekordy
5.
Impact of environmental conditions in West Europe, Poland and Algeria on outdoor insulators performance and selection / Chrzan, K L ; Abdi, S E [I07/2007/I-045] [ENY-ARTICLE-2008-192]
This paper presents the data of environmental conditions in France, Germany, Poland and Algeria. [...]
http://zet10.ipee.pwr.wroc.pl/record/246/files/
Rekord szczegółowy - Podobne rekordy
6.
Mechanical-Acoustic Examination of Ceramic Material / Ranachowski, P ; Rejmund, F [ENY-ARTICLE-2008-126]
The paper presents a new mechanical-acoustic method of research of material degradation. [...]
http://zet10.ipee.pwr.wroc.pl/record/164/files/
Rekord szczegółowy - Podobne rekordy
7.
Influence of pollution layer thickness on flashover voltage of HV insulators / Wankowicz, J ; Chrzan, K L ; Pohl, Z [ENY-ARTICLE-2012-325]
The pollution characteristics (the relationships of flashover voltage and SDD or maximum current Imax ) for insulators contaminated with uniform or nonuniform coatings with different thickness h are presented. [...]
http://zet10.ipee.pwr.wroc.pl/record/412/files/
Rekord szczegółowy - Podobne rekordy

Jeżeli nie znaleziono tego czego szukasz, spróbuj szukać na innych serwerach:
recid:436 w Google Books
recid:436 w Google Scholar
recid:436 w Google Web
recid:436 w INSPEC